Precision Alloy 32N14K
It is used in parts of high precision instruments requiring dimensional stability in the range of climatic temperatures.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precision alloys |
Soft Magnetic Precision Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Co, % |
Ti, % |
Cu, % |
Ni, % |
Al, % |
ET, % |
| GOST 10994-74 |
51.91–55 |
< 0.3 |
< 0.4 |
13.5–14.5 |
< 0.1 |
< 0.2 |
31.5–32.5 |
< 0.02 |
< 0.07 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\alpha\cdot 10^{6}$$, $$K^{-1}$$ |
$$\varkappa$$, $$\frac{W}{m\cdot K}$$ |
$$\rho$$, $$\frac{kg}{m^3}$$ |
Cp, Дж/кг·К |
| 20 |
12–17 |
56–75 |
8100 |
456 |
Mechanical properties at 20 °C
| Rolling |
Standard |
Size, mm |
Tension |
Classifiers |
$$\sigma _{U}$$, $$MPa$$ |
$$\sigma_{Y}$$, $$MPa$$ |
d5, % |
Treatment |
| Tape |
GOST 10994-74 |
100 |
Transverse |
|
460–480 |
190–210 |
30–35 |
|
Brinell hardness number
| Rolling |
Standard |
Classifiers |
Value, HBW |
| Tape |
GOST 10994-74 |
|
90–100 |
Casting and technological parameters
Limit operating modes
Wärmebehandlungsmodi
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Co |
% |
Cobalt |
| Ti |
% |
Titan |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| Cp |
Дж/кг·К |
Specific heat of material |
| $$\alpha\cdot 10^{6}$$ |
$$K^{-1}$$ |
Coefficient of thermal (linear) expansion (range 20°C–T) |
| $$\varkappa$$ |
$$\frac{W}{m\cdot K}$$ |
Coefficient of thermal conductivity (the heat capacity of the material) |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of mechanical properties
| Parameter |
Units of measurement |
Description |
| d5 |
% |
Elongation at break |
| $$\sigma_{Y}$$ |
$$MPa$$ |
Yield strength |
| $$\sigma _{U}$$ |
$$MPa$$ |
Ultimate tensile strength |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |