FVd50U0.3
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cu, % |
V, % |
Al, % |
As, % |
P, % |
C, % |
S, % |
| GOST 27130-94 |
44.55–50 |
< 2 |
< 0.2 |
< 0.2 |
44.55–55.45 |
< 2.5 |
< 0.05 |
< 0.1 |
< 0.3 |
< 0.1 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| V |
% |
Vanadium |
| Al |
% |
Aluminium |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |