LAMSH77-2-0.04
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
As, % |
P, % |
ET, % |
| GOST 15527-2004 |
< 0.1 |
< 0.002 |
76–79 |
< 17.48 |
< 0.5 |
< 0.005 |
1.7–2.5 |
< 0.07 |
0.02–0.04 |
< 0.01 |
< 0.3 |
Information on suppliers
Analogues
| Germany |
USA |
| SoMs76 |
SB 111 (C68700) |