LANKMts75-2-2.5-0.5-0.5
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Si, % |
Bi, % |
Mn, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Al, % |
Pb, % |
P, % |
ET, % |
| GOST 15527-2004 |
< 0.1 |
0.3–0.7 |
< 0.002 |
0.3–0.7 |
73–76 |
16.733–22.8 |
2–3 |
< 0.005 |
1.6–2.2 |
< 0.05 |
< 0.01 |
< 0.5 |
Information on suppliers
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| ET |
% |
Total other items |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Bi |
% |
Bismuth |
| Mn |
% |
Manganese |
| Cu |
% |
Copper |
| Zn |
% |
Zinc |
| Ni |
% |
Nickel |
| Sb |
% |
Antimony |
| Al |
% |
Aluminium |
| Pb |
% |
Lead |
| P |
% |
Phosphorus |