LMSh68-0.05
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Zn, % |
Ni, % |
Sb, % |
Pb, % |
As, % |
P, % |
Примеси, % |
| GOST 15527-2004 |
< 0.1 |
< 0.002 |
67–70 |
28.993–32.98 |
< 0.5 |
< 0.005 |
< 0.03 |
0.02–0.06 |
< 0.01 |
< 0.3 |
Information on suppliers
Analogues
| USA |
Germany |
| B 569 (C26130) |
Ms70 |