PSR 25
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Zn, % |
Pb, % |
Ag, % |
Примеси, % |
| GOST 19738 - 2015 |
< 0.1 |
< 0.005 |
38.095–41.905 |
33.395–36.3 |
< 0.05 |
24.7–25.3 |
< 0.15 |