Wood Alloy
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Sn, % | Bi, % | Pb, % | Cd, % |
|---|---|---|---|---|
| TU 6-09-4064-87 | 8.85–9.75 | 39.3–40.2 | 40.3–43 | 8.85–9.75 |
Information on suppliers
Analogues
| USA |
|---|
| Roto158F |
Standards
| Standard | Description |
|---|---|
| TU 6-09-4064-87 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Sn | % | Tin |
| Bi | % | Bismuth |
| Pb | % | Lead |
| Cd | % | Cadmium |