Sprabond
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Si, % | Ni, % | Al, % | C, % | O, % | Mo, % |
|---|---|---|---|---|---|---|---|
| TU 48-19-290-91 | < 0.01 | < 0.001 | < 0.005 | < 0.004 | < 0.005 | < 0.008 | > 99.967 |
Note: Ca + Mg <0.005
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 48-19-290-91 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Ni | % | Nickel |
| Al | % | Aluminium |
| C | % | Carbon |
| O | % | Oxygen |
| Mo | % | Molybdenum |