Sr99.99An
For the manufacture of silver anodes intended for electroplating silver articles
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Silver |
Chemical composition
| Standard | Fe, % | Bi, % | Mn, % | Cu, % | Sb, % | Te, % | Pb, % | Ag, % | Pd, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 25474-2015 | < 0.002 | < 0.0005 | < 0.001 | < 0.008 | < 0.001 | < 0.002 | < 0.001 | > 99.99 | < 0.001 |
Information on suppliers
Physical characteristics
| Temperature, °C | $$\rho$$, $$\frac{kg}{m^3}$$ |
|---|---|
| 20 | 10500 |
Standards
| Standard | Description |
|---|---|
| GOST 25474-2015 | GOST |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Cu | % | Copper |
| Sb | % | Antimony |
| Te | % | Tellurium |
| Pb | % | Lead |
| Ag | % | Silver |
| Pd | % | Palladium |
Description of physical characteristics
| Parameter | Units of measurement | Description |
|---|---|---|
| $$\rho$$ | $$\frac{kg}{m^3}$$ | The density of the material |