CpA 1 (999.9m)
Refined silver.
Production of ingots designed for the needs of the national economy and export
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Precious metals | Silver |
Chemical composition
| Standard | Fe, % | Bi, % | Sb, % | Te, % | Pb, % | Ag, % | Au, % |
|---|---|---|---|---|---|---|---|
| GOST 28595-2015 | < 0.001 | < 0.001 | < 0.001 | < 0.002 | < 0.002 | > 99.99 | < 0.0006 |
Information on suppliers
Analogues
| USA |
|---|
| B 413 Grade 99.99 |
Standards
| Standard | Description |
|---|---|
| GOST 28595-2015 | GOST |
| GOST 28595-90 |