SRKdin 72.5
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | B, % | Ni, % | Cd, % | Ag, % | In, % |
|---|---|---|---|---|---|
| TU 117-1-799-92 | < 0.02 | 0.04–0.08 | 25.9–27.5 | 71.4–73.56 | 0.5–1 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 117-1-799-92 | |
| TU 48-1-777-86 | |
| TU 48-1-792-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| B | % | Bor |
| Ni | % | Nickel |
| Cd | % | Cadmium |
| Ag | % | Silver |
| In | % | Indium |