SRM 75
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Corrosion-resistant alloys and steels |
Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Sb, % |
Pb, % |
Ag, % |
Примеси, % |
| GOST 24552-14 |
< 0.13 |
< 0.002 |
24.221–25.5 |
< 0.002 |
< 0.005 |
74.221–75.779 |
< 0.14 |