SrM80 (SRM 800)
Silver-copper alloy. Melting point: 779 — 810 ° C
For the manufacture of sliding contacts, electrical conductors and other products and technical purposes.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precious metals |
Silver, silver alloys |
Chemical composition
| Standard |
Fe, % |
Bi, % |
Cu, % |
Sb, % |
Pb, % |
Ag, % |
| GOST 6836-2002 |
< 0.13 |
< 0.002 |
19.42–20.16 |
< 0.002 |
< 0.005 |
79.7–80.3 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
10130 |
Casting and technological parameters
| melting point, °C |
| 779–810 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Bi |
% |
Bismuth |
| Cu |
% |
Copper |
| Sb |
% |
Antimony |
| Pb |
% |
Lead |
| Ag |
% |
Silver |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |