SrMgN 99
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Mg, % | Ni, % | Ag, % |
|---|---|---|---|
| TU 117-1-259-92 | 0.15–0.32 | 0.1–0.15 | 99.53–99.75 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 117-1-259-92 | |
| TU 117-1-260-92 | |
| TU 117-1-285-92 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Mg | % | Magnesium |
| Ni | % | Nickel |
| Ag | % | Silver |