SRNMin 78
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Cu, % | Ni, % | Ag, % | In, % |
|---|---|---|---|---|
| TU 117-1-392-94 | 18.2–21.8 | 0.5–1.5 | 75.4–80.6 | 0.7–1.3 |