SrPL-4 (SrPl 96−4)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Fe, % | Pb, % | Ag, % | Pt, % | Pd, % | Примеси, % |
|---|---|---|---|---|---|---|
| GOST 6836-80 | < 0.03 | < 0.005 | 95.235–96.4 | 3.6–4.4 | < 0.15 | < 0.18 |
Note: Pd: Pd + Ir + Rh + Au
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 6836-80 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Примеси | % | Impurities |
| Pb | % | Lead |
| Ag | % | Silver |
| Pt | % | Platinum |
| Pd | % | Palladium |