SrPl96-4 (SrPL-4)
Silver-platinum alloy. Melting point: 960 — 1000 ° C
For the manufacture of discontinuous and sliding contacts, as well as other products and technical purposes.
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Precious metals |
Silver, silver alloys |
Chemical composition
| Standard |
Fe, % |
Pb, % |
Ag, % |
Pt, % |
| GOST 6836-2002 |
< 0.03 |
< 0.005 |
95.6–96.4 |
3.6–4.4 |
Information on suppliers
Physical characteristics
| Temperature, °C |
$$\rho$$, $$\frac{kg}{m^3}$$ |
| 20 |
10720 |
Casting and technological parameters
| melting point, °C |
| 960–1000 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Pb |
% |
Lead |
| Ag |
% |
Silver |
| Pt |
% |
Platinum |
Description of physical characteristics
| Parameter |
Units of measurement |
Description |
| $$\rho$$ |
$$\frac{kg}{m^3}$$ |
The density of the material |
Description of the casting and technological parameters
| Parameter |
Units of measurement |
Description |
| melting point |
°C |
The temperature at which solid crystalline body makes the transition to the liquid state and Vice versa |