SSu8
for the production of batteries, corrosion-resistant equipment and the chemical industry
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Tin, lead, babity | Lead antimony alloys |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Cu, % | Zn, % | Sb, % | Pb, % | As, % |
|---|---|---|---|---|---|---|---|---|
| GOST 1292-81 | < 0.005 | < 0.01 | < 0.03 | < 0.002 | < 0.002 | 7–8.5 | 91.476–93 | < 0.005 |