SSZP-1
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Corrosion-resistant alloys and steels | Corrosion-resistant heat-resistant steel |
Chemical composition
| Standard | Te, % | Pb, % | Ag, % | Au, % | Pt, % | Se, % | Примеси, % |
|---|---|---|---|---|---|---|---|
| TU 117-2-2-90 | < 0.1 | < 0.3 | > 87.8 | < 10 | < 0.2 | < 0.1 | < 1.5 |
Note: Pt: Pt + Pd + Rh
Note: OT: OT + Se + Te + Pb
Information on suppliers
Standards
| Standard | Description |
|---|---|
| TU 117-2-2-90 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Примеси | % | Impurities |
| Te | % | Tellurium |
| Pb | % | Lead |
| Ag | % | Silver |
| Au | % | Gold |
| Pt | % | Platinum |
| Se | % | Selenium |