CT-1
For glass, paints, enamels, to obtain pure selenium and other purposes
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Selenium |
Chemical composition
| Standard | Fe, % | Cu, % | Al, % | Te, % | Pb, % | As, % | S, % | Se, % | Hg, % |
|---|---|---|---|---|---|---|---|---|---|
| GOST 10298-79 | < 0.01 | < 0.005 | < 0.005 | < 0.1 | < 0.005 | < 0.005 | < 0.02 | < 99 | < 0.005 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 10298-79 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Cu | % | Copper |
| Al | % | Aluminium |
| Te | % | Tellurium |
| Pb | % | Lead |
| As | % | Arsenic |
| S | % | Sulfur |
| Se | % | Selenium |
| Hg | % | Mercury |