Heat resisting structural steel 20X25H19S2L
Designed for the manufacture of castings for furnace equipment operating at operating temperatures up to 1000 degrees. WITH
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant high alloy steel |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 977-88 |