Heat-resistant alloyed structural steel 20X25N20SL
Shaped castings are used to obtain parts of high-temperature equipment for oil refining and petrochemical industries
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Heat resistant steels and alloys | Heat resistant high alloy steel |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 977-88 | |
| TU 4112-161-00220302-2011 | TU 4112-161-00220302-2011 |