Su00
It is used for the manufacture of solder on the tin-lead-based, enamel and ceramic pigments
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Antimony |
Chemical composition
| Standard | Fe, % | Sn, % | Bi, % | Zn, % | Ni, % | Sb, % | Pb, % | As, % | S, % | Au, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1089 - 82 | < 0.01 | < 0.02 | < 0.004 | < 0.005 | < 0.008 | > 99.9024 | < 0.03 | < 0.01 | < 0.01 | < 0.0006 |