Su000
It is used for the production of antimony brand Su0000P and special solders
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Antimony |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Bi, % | Mn, % | Cu, % | Zn, % | Ni, % | Sb, % | Pb, % | As, % | Cd, % | S, % | Ag, % | Au, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1089 - 82 | < 0.0004 | < 0.0005 | < 0.0001 | < 4.0E-5 | < 0.0002 | < 5.0E-5 | < 0.0005 | < 0.0002 | > 99.9959 | < 0.0006 | < 0.0004 | < 0.0002 | < 0.0005 | < 1.0E-5 | < 0.0004 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1089 - 82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| Cd | % | Cadmium |
| S | % | Sulfur |
| Ag | % | Silver |
| Au | % | Gold |