Su0000P
It is used in semi-conductor technology
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Antimony |
Chemical composition
| Standard | Fe, % | Si, % | Sn, % | Mg, % | Bi, % | Mn, % | Cu, % | Zn, % | Ni, % | Sb, % | Te, % | Na, % | Pb, % | As, % | Cd, % | S, % | Ag, % | Au, % | Se, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| GOST 1089 - 82 | < 2.0E-5 | < 4.0E-5 | < 3.0E-5 | < 2.0E-5 | < 2.0E-5 | < 3.0E-6 | < 5.0E-6 | < 5.0E-5 | < 2.0E-5 | > 99.999488 | < 1.0E-5 | < 0.0001 | < 1.0E-5 | < 3.0E-5 | < 2.0E-6 | < 5.0E-5 | < 2.0E-6 | < 5.0E-5 | < 5.0E-5 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1089 - 82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Sn | % | Tin |
| Mg | % | Magnesium |
| Bi | % | Bismuth |
| Mn | % | Manganese |
| Cu | % | Copper |
| Zn | % | Zinc |
| Ni | % | Nickel |
| Sb | % | Antimony |
| Te | % | Tellurium |
| Na | % | Sodium |
| Pb | % | Lead |
| As | % | Arsenic |
| Cd | % | Cadmium |
| S | % | Sulfur |
| Ag | % | Silver |
| Au | % | Gold |
| Se | % | Selenium |