Cy1
It used for the manufacture of anti-friction, storage, printing alloys and alloys for the cable sheath
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Metals and alloys | Antimony |
Chemical composition
| Standard | Fe, % | Sn, % | Sb, % | Pb, % | As, % | S, % |
|---|---|---|---|---|---|---|
| GOST 1089 - 82 | < 0.1 | < 0.08 | > 99.52 | < 0.1 | < 0.1 | < 0.1 |
Information on suppliers
Standards
| Standard | Description |
|---|---|
| GOST 1089 - 82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Sn | % | Tin |
| Sb | % | Antimony |
| Pb | % | Lead |
| As | % | Arsenic |
| S | % | Sulfur |