Sv-20H27N6M3AGV

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Wrought Aluminum Alloys

Chemical composition

Standard Fe, % Si, % Ca, % Mn, % Cr, % Ni, % Ce, % P, % C, % S, % Y, % Mo, % N, % W, %
TU 14-1-3376-82 58.155–65 < 0.5 < 0.1 1–2 26–28 5–7 < 0.1 < 0.025 0.15–0.25 < 0.02 < 0.1 2.5–3 0.15–0.25 0.2–0.5

Information on suppliers

Свойства

Свойство
Вычисляемые свойства Плотность: 7.79 г/см3

Standards

Standard Description
TU 14-1-3376-82