Sv-01X12H2MT-VI (EP-959-VI)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| TU 14-1-3595-83 |
82.52–85.41 |
0.25–0.5 |
< 0.2 |
12–13.5 |
0.04–0.12 |
1.7–2.2 |
< 0.015 |
< 0.01 |
< 0.015 |
0.6–0.9 |
< 0.02 |
Information on suppliers
Properties
| Property |
| Density: 7.8 g/cm3 |
Analogues
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |