SV-01Х12Н4Б (ЭП909)
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|---|---|
| OST 24.300.04-91 | 82.62–87.05 | 0.15–0.55 | 0.2–0.75 | 11–13.5 | 1.6–2.5 | < 0.025 | < 0.035 | < 0.02 |
Note: The weld metal
Note: Automatic welding under flux
Information on suppliers
Свойства
| Свойство |
|---|
| Плотность: 7.79 г/см3 |
Standards
| Standard | Description |
|---|---|
| OST 24.300.04-91 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |