Sv-01H25N19G5AM4 (ChS84)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
|
42.75–49.85 |
0.25 |
4–6 |
25–27 |
18–20 |
0.018 |
0.025 |
0.015 |
3–4 |
0.15–0.25 |
Information on suppliers
Properties
| Property |
| Density: 7.92 g/cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |