Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
Zr, % |
Al, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-3013-80 |
73.767–75.9 |
1.4–1.7 |
< 0.003 |
0.6–0.9 |
11.6–12 |
0.2–0.3 |
8.5–8.9 |
< 0.08 |
< 0.1 |
< 0.01 |
< 0.03 |
< 0.01 |
1.8–2.2 |
Information on suppliers
Properties
| Property |
| Density: 7.83 g/cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Zr |
% |
Zirconium |
| Al |
% |
Aluminium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |