SV-03Х19Н15Г6М2АВ2 (ChS39)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
W, % |
| TU 14-1-1588-76 |
50–56.55 |
< 0.2 |
6–7.5 |
18–20 |
15–16.5 |
< 0.04 |
< 0.03 |
< 0.01 |
2.5–3.2 |
0.15–0.22 |
1.8–2.3 |
Information on suppliers
Свойства
| Свойство |
| Плотность: 8.15 г/см3 |