Sv-03H23N28M3D3T

Classification

Country Section Category
CIS, Russia, Ukraine Materials for welding and soldering Steel welding wire

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Ti, % Cu, % Ni, % P, % C, % S, % Nb, % Mo, %
TU 14-1-2571-78 38.187–46.4 < 0.25 1.5–2.5 22–25 < 0.1 2.5–3 24.5–27 < 0.02 < 0.025 < 0.018 0.6–0.9 2.5–3

Information on suppliers

Eigenschaften

Eigenschaft
Dichte: 8.06 G/cm3

Analogues

Germany USA
X 1 NiCrMoCuN 25-20-7 INCO alloy 904L

Standards

Standard Description
OST 26-291-94
TU 14-1-2571-78

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Cr % Chrome
Ti % Titan
Cu % Copper
Ni % Nickel
P % Phosphorus
C % Carbon
S % Sulfur
Nb % Niobium
Mo % Molybdenum