Св-03ХН25МДГ (03HN25MDG)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| TU 14-1-2571-78 |
38.487–47 |
< 0.25 |
1.5–2.5 |
22–25 |
< 0.1 |
2.5–3.5 |
24.5–27 |
< 0.02 |
< 0.025 |
< 0.018 |
< 0.1 |
2.5–3 |
Information on suppliers
Свойства
| Свойство |
| Плотность: 8.05 г/см3 |