Sv-04N3GMTA
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
P, % |
C, % |
S, % |
O, % |
Mo, % |
N, % |
| TU 14-105-596-96 |
94.583–96.05 |
< 0.2 |
1.3–1.6 |
< 0.3 |
0.05–0.12 |
2.4–2.8 |
< 0.015 |
< 0.05 |
< 0.012 |
< 0.005 |
0.2–0.3 |
< 0.015 |
Information on suppliers
Properties
| Property |
| Wire rod for welding wire according to TU 14-105-596-96 Temporary resistance: <690 MPa Relative narrowing:> 48% |
| Wire according to TU 5.965-11610-96 Nominal diameter: 4 mm; Temporary resistance: 800 - 1250 MPa |
| Density: 7.88 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| O |
% |
Oxygen |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |