Sv-05H30N40M6TB
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
P, % |
C, % |
S, % |
Nb, % |
Mo, % |
| TU 14-1-914-74 |
16.925–25.2 |
0.3–0.6 |
1–2 |
28–30 |
< 0.6 |
33.725–47.275 |
< 0.02 |
< 0.05 |
< 0.005 |
0.5–0.8 |
6–7 |
Information on suppliers
Properties
| Property |
| Density: 8.2 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Nb |
% |
Niobium |
| Mo |
% |
Molybdenum |