Sv-06H24N6TAFM (EP401)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
V, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| TU 14-1-2549-78 |
65.702–71.252 |
< 0.7 |
< 0.8 |
23–25.5 |
0.08–0.2 |
5.5–6.5 |
0.008–0.15 |
< 0.03 |
< 0.08 |
< 0.018 |
0.06–0.12 |
0.1–0.2 |
Information on suppliers
Properties
| Property |
| Density: 7.72 g / cm3 |