Sv-07H22N13G5ST (ChS49)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Ca, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
Al, % |
Ce, % |
P, % |
C, % |
S, % |
Y, % |
| TU 14-1-2646-79 |
52.731–61 |
0.8–1.2 |
< 0.004 |
< 0.01 |
5–6 |
21–23 |
0.2–0.5 |
12–14 |
< 2.2 |
< 0.2 |
< 0.02 |
< 0.07 |
< 0.015 |
< 0.05 |
Information on suppliers
Properties
| Property |
| Density: 7.64 g / cm3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| B |
% |
Bor |
| Ca |
% |
Calcium |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| Ce |
% |
Cerium |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Y |
% |
Yttrium |