Sv-07H25N13U
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Materials for welding and soldering |
Steel welding wire |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
| OST 24.300.04-91 |
57.087–62.5 |
0.5–0.8 |
1.5–2 |
23.5–26 |
12–14 |
< 0.018 |
< 0.08 |
< 0.015 |
Information on suppliers
Properties
| Property |
| Density: 7.79 g / cm3 |