Sv-07PNMAA
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
Al, % |
As, % |
P, % |
C, % |
S, % |
Mo, % |
N, % |
| TU У 14-16-130-97 |
95.795–97.7 |
0.2–0.45 |
1–1.5 |
< 0.3 |
< 0.2 |
0.5–0.7 |
< 0.05 |
< 0.05 |
< 0.01 |
< 0.08 |
< 0.005 |
0.6–0.85 |
< 0.01 |
Information on suppliers
Свойства
| Свойство |
| Проволока сварочная по ТУ У 14-16-130-97 Временное сопротивление: 70 - 95 МПа |
| Плотность: 7.87 г/см3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Cu |
% |
Copper |
| Ni |
% |
Nickel |
| Al |
% |
Aluminium |
| As |
% |
Arsenic |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| Mo |
% |
Molybdenum |
| N |
% |
Nitrogen |