St-08AA
Welding cold drawn wire of low carbon steel welding (surfacing), and the manufacture of electrodes
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Materials for welding and soldering | Steel welding wire |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | Al, % | P, % | C, % | S, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2246-70 | 98.862–99.65 | < 0.03 | 0.35–0.6 | < 0.1 | < 0.25 | < 0.01 | < 0.02 | < 0.1 | < 0.02 | < 0.008 |
Information on suppliers
Properties
| Property |
|---|
| According to TU 0934-002-55791017-2010 Diameter: 5.5 - 7.0 mm; Temporary resistance: <420 MPa Relative narrowing:> 55% |
| Density: 7.86 g / cm3 |
Analogues
| Germany |
|---|
| 1.1116 (USD6) |
Standards
| Standard | Description |
|---|---|
| GOST 2246-70 | |
| TU 0934-002-55791017-2010 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| Al | % | Aluminium |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| N | % | Nitrogen |