Sv-08G1NMA
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ti, % | Ni, % | V, % | Al, % | As, % | P, % | C, % | S, % | Mo, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| TU 1200-053-00187240-2010 | 96.046–97.59 | 0.2–0.4 | 1.3–1.8 | < 0.3 | < 0.04 | 0.35–0.5 | < 0.05 | < 0.05 | < 0.04 | < 0.012 | 0.06–0.09 | < 0.01 | 0.5–0.65 | < 0.012 |
Note: N> 0.010 - as agreed
Information on suppliers
Properties
| Property |
|---|
| According to TU 1200-053-00187240-2010 Temporary resistance: 588 - 784 MPa |
| Density: 7.86 g / cm3 |
Standards
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ti | % | Titan |
| Ni | % | Nickel |
| V | % | Vanadium |
| Al | % | Aluminium |
| As | % | Arsenic |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Mo | % | Molybdenum |
| N | % | Nitrogen |