Sv-08g1sa

Classification

Country Section Category
CIS, Russia, Ukraine Aluminum, aluminum alloys Wrought Aluminum Alloys

Chemical composition

Standard Fe, % Si, % Mn, % Cr, % Cu, % Ni, % P, % C, % S, % N, %
TU У 14-4-495-2001 96.293–97.74 0.8–1.1 1.4–1.7 < 0.2 < 0.25 < 0.3 < 0.02 0.06–0.11 < 0.02 < 0.007

Note: + B

Information on suppliers

Eigenschaften

Eigenschaft
Draht nach TU U 14-4-495-2001 Temporärer Widerstand: <560 MPa Relative Verengung:> 65%
Dichte: 7,81 g / cm³

Analogues

Germany USA
1.5125 K11140

Standards

Standard Description
TU У 14-4-495-2001

Description of chemical elements

Element Units of measurement Description
Fe % Iron
Si % Silicon
Mn % Manganese
Cr % Chrome
Cu % Copper
Ni % Nickel
P % Phosphorus
C % Carbon
S % Sulfur
N % Nitrogen