Sv-08g1sr
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
P, % |
C, % |
S, % |
N, % |
| TU У 14-4-486-2000 |
97.383–97.945 |
0.75–0.85 |
0.005–0.01 |
1.3–1.6 |
< 0.02 |
< 0.11 |
< 0.02 |
< 0.007 |
Information on suppliers
Свойства
| Свойство |
| Сварочная проволока Временное сопротивление: < 560 МПа Относительное удлинение: < 65 % |
| Плотность: 7.82 г/см3 |
| Примечание Катанка |