Sv-08g2s-o
Classification
| Country | Section | Category |
|---|---|---|
| CIS, Russia, Ukraine | Aluminum, aluminum alloys | Wrought Aluminum Alloys |
Chemical composition
| Standard | Fe, % | Si, % | Mn, % | P, % | C, % | S, % |
|---|---|---|---|---|---|---|
| TU 14-178-220-99 | 96.785–97.45 | 0.7–0.95 | 1.8–2.1 | < 0.03 | 0.05–0.11 | < 0.025 |
Note: With the consent of the consumer, in a wire with a diameter of up to 1.4 mm, the mass fraction of Mn: 1.65 - 2.1%
Note: According to customer demand Cu <0.2%
Note: By agreement with the consumer N <0.012%
Note: The copper content should not exceed 0.3%, taking into account the copper contained in the coating
Information on suppliers
Properties
| Property |
|---|
| Density: 7.81 g / cm3 |
Analogues
| European Union |
|---|
| G4Si1 |
Standards
| Standard | Description |
|---|---|
| TU 14-178-220-99 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |