Sv-08G2SNTUR
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
B, % |
Mn, % |
Cr, % |
Ti, % |
Cu, % |
Ni, % |
Al, % |
P, % |
C, % |
S, % |
| OST 26-291-94 |
94.3–96.54 |
0.35–0.6 |
< 0.005 |
1.7–2.2 |
< 0.3 |
0.15–0.4 |
< 0.025 |
1–1.4 |
0.2–0.6 |
< 0.03 |
0.06–0.11 |
< 0.03 |
Information on suppliers
Свойства
| Свойство |
| Плотность: 7.81 г/см3 |