Sv-08GSNTA
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ti, % |
Ni, % |
P, % |
C, % |
S, % |
O, % |
N, % |
| TU 14-105-596-96 |
95.583–97.15 |
0.6–0.9 |
1.4–1.8 |
< 0.3 |
0.05–0.12 |
0.8–1.2 |
< 0.015 |
< 0.05 |
< 0.012 |
< 0.005 |
< 0.015 |
Information on suppliers
Свойства
| Свойство |
| Катанка для сварочной проволоки по ТУ 14-105-596-96 Временное сопротивление: < 690 МПа Относительное сужение: > 48 % |
| Плотность: 7.83 г/см3 |
Standards
Description of chemical elements
| Element |
Units of measurement |
Description |
| Fe |
% |
Iron |
| Si |
% |
Silicon |
| Mn |
% |
Manganese |
| Cr |
% |
Chrome |
| Ti |
% |
Titan |
| Ni |
% |
Nickel |
| P |
% |
Phosphorus |
| C |
% |
Carbon |
| S |
% |
Sulfur |
| O |
% |
Oxygen |
| N |
% |
Nitrogen |