Sv-08X14H8S3B (EP305)
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Ni, % |
P, % |
C, % |
S, % |
Nb, % |
| TU 14-1-1890-76 |
68.757–73.35 |
2.8–3.5 |
1.5–2 |
13.5–15.5 |
8–9 |
< 0.025 |
0.05–0.1 |
< 0.018 |
0.8–1.1 |
Information on suppliers
Properties
| Property |
| Density: 7.68 g / cm3 |