Sv-08X17H5M3
Classification
| Country |
Section |
Category |
| CIS, Russia, Ukraine |
Aluminum, aluminum alloys |
Wrought Aluminum Alloys |
Chemical composition
| Standard |
Fe, % |
Si, % |
Mn, % |
Cr, % |
Cu, % |
Ni, % |
P, % |
C, % |
S, % |
Mo, % |
| TU 14-1-997-2012 |
71.545–76.44 |
< 0.8 |
< 0.8 |
16–17.5 |
< 0.2 |
4.5–5.5 |
< 0.035 |
0.06–0.1 |
< 0.02 |
3–3.5 |
Information on suppliers
Свойства
| Свойство |
| По ТУ 14-1-997-2012 Примечание Механические свойства не нормируются Механические свойства: по согласованию |
| Плотность: 7.85 г/см3 |