Chemical composition
| Standard | Fe, % | Si, % | Mn, % | Cr, % | Ni, % | P, % | C, % | S, % | Nb, % | N, % |
|---|---|---|---|---|---|---|---|---|---|---|
| GOST 2246-70 | 64.85–69.05 | 0.2–0.45 | 1.8–2.2 | 18.5–20.5 | 9.5–10.5 | < 0.03 | 0.05–0.1 | < 0.02 | 0.9–1.3 | < 0.05 |
Information on suppliers
Properties
| Property |
|---|
| Note Fluctuations in the tensile strength in one coil of wire with a diameter of more than 1.4 mm should not exceed 90 N / mm2. |
| For welding Diameter: 0.3 - 0.5 mm; Temporary resistance: 890 - 1390 MPa |
| Diameter: 0.8 - 1.5 mm; Temporary resistance: 890 - 1340 MPa |
| Diameter: 1.6mm; Temporary resistance: 890 - 1290 MPa |
| Diameter: 2mm; Temporary resistance: 790 - 1190 MPa |
| Diameter:> 2 mm; Temporary resistance: 690 - 1040 MPa |
| For the manufacture of electrodes Diameter: 1.6 mm; Temporary resistance: 690 - 990 MPa |
| Diameter: 2mm; Temporary resistance: 690 - 990 MPa |
| Diameter:> 2 mm; Temporary resistance: 640 - 940 MPa |
| Density: 7.82 g / cm3 |
Analogues
| Germany | USA |
|---|---|
| 347 | W34740 |
Standards
| Standard | Description |
|---|---|
| GOST 2246-70 | |
| OST 24.300.04-91 | |
| TU 14-1-3349-82 |
Description of chemical elements
| Element | Units of measurement | Description |
|---|---|---|
| Fe | % | Iron |
| Si | % | Silicon |
| Mn | % | Manganese |
| Cr | % | Chrome |
| Ni | % | Nickel |
| P | % | Phosphorus |
| C | % | Carbon |
| S | % | Sulfur |
| Nb | % | Niobium |
| N | % | Nitrogen |